japanese metallic yarn,st type metallic yarn
Type | Width | Thickness | Composition(aprx) | Length/kg | Nm | Denier | package |
ST | 1/64” | 12Mir | M:38%,VS/150D:62% | 38,000M+-3% | 38 | 237D | 125gms |
500gms |
japanese metallic yarn,st type metallic yarn
1.PURE GOLD metaLLIC YARN
2.CORE IS RAYON VISCOSE 150D
3.PACKING IS 125GMS/CONE OR 250GMS/CONE OR 500GMS/CONE
Laundry | 0.5%(5gr./liter) soap 60°C 20min | O |
Dry cleaning | Petroleum benzine 100% 20 °C 30min. perchlorethylene 100% 20 °C 30min. trichloethylne 100% 20 °C 30min. | O |
Ironing | 135°C 15sec. | O |
Hot water | 70°C 30min. | O |
Steam | 100°C 10min. | O |
Dry heating | 100°C 60sec. | O |
Scouring for nylon,polyester rayon,acetate&cotton | soap 0.5gr./liter,soda ash 0.5gr/liter 80°C 30min | X |
For wool | monogen 5.0gr./liter, 60°C 30min. | O |
Overdye wool&nylon nylon and acetate | acetic acid 2.0gr./liter, 60°C 120min. | X |
Bleaching | sodium hydrosulfite 2.0gr./liter,80°C 60min soda 0.5gr./liter,80°C 60min
ph 9 30% hydrogen peroxide 40gr./liter, 70°C 60min. 10% sodium hydrochlorite 40gr./liter, 70°C 60min. | X |
Finishing | sodium carbonate ph 9 95°C 60min | X |
Caustic soda | 28 Be' 21°C sec. | X
|